Influence of Quench Rate on the Artificial Ageing Response of an Al-8Si-0.4Mg Cast Alloy
Högskolan i Jönköping, Tekniska Högskolan, JTH. Forskningsmiljö Material och tillverkning – Gjutning. Scania AB.
Högskolan i Jönköping, Tekniska Högskolan, JTH. Forskningsmiljö Material och tillverkning – Gjutning.ORCID-id: 0000-0001-6481-5530
University of Padova.
2015 (engelsk)Inngår i: Materials Science Forum, ISSN 0255-5476, E-ISSN 1662-9752, Vol. 828-829, s. 219-225Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

The aim of the study is to present the influence of quench rate on the artificial ageing response of Al-8%Si-0.4%Mg cast alloy in terms of Brinell hardness and yield strength. The investigated material was produced by a gradient solidification technique and exhibited a microstructure that corresponds to the one of gravity die castings, with a dendrite arm spacing of approximately 25 μm. The study comprises two solution treatment temperatures, five quench rates and artificial ageingtimes exceeding 100 hours at 170 and 220 ⁰C. The microstructure and concentration profiles of Mgand Si were evaluated using energy and wavelength dispersive spectroscopy. Microstructural examination reveals an increment of solutes in the Al-matrix when higher solution treatment temperatures accompanied with high quench rates are applied and shows how both Si and Mgatoms have diffused towards the eutectic during quenching. Consequently, i.e. by increasing the levels of solutes and vacancies, the highest strength levels were realized. The study confirmed that quench rates above 2 ⁰C /s do not offer substantial strength improvement while quenching at lower rates resulted in a lower peak hardness and longer times to peak.

sted, utgiver, år, opplag, sider
Trans Tech Publications, 2015. Vol. 828-829, s. 219-225
Emneord [en]
Al-Si cast alloys, Solution heat treatment, Quench rates, Ageing, Hardness
HSV kategori
Identifikatorer
URN: urn:nbn:se:hj:diva-27142DOI: 10.4028/www.scientific.net/MSF.828-829.219Scopus ID: 2-s2.0-84954527841Lokal ID: JTHMaterialISOAI: oai:DiVA.org:hj-27142DiVA, id: diva2:820408
Tilgjengelig fra: 2015-06-12 Laget: 2015-06-12 Sist oppdatert: 2018-10-16bibliografisk kontrollert

Open Access i DiVA

fulltext(419 kB)450 nedlastinger
Filinformasjon
Fil FULLTEXT01.pdfFilstørrelse 419 kBChecksum SHA-512
4b89e01efbfa7e7f244e1602378dae7d3ad1cb39dc57bb616e0de666cd66dfdb091da9483e57edb789cf4a1e0621fdfa98e8da9dffc946582ec4683d707d915a
Type fulltextMimetype application/pdf

Andre lenker

Forlagets fulltekstScopus

Person

Seifeddine, Salem

Søk i DiVA

Av forfatter/redaktør
Seifeddine, Salem
Av organisasjonen
I samme tidsskrift
Materials Science Forum

Søk utenfor DiVA

GoogleGoogle Scholar
Totalt: 450 nedlastinger
Antall nedlastinger er summen av alle nedlastinger av alle fulltekster. Det kan for eksempel være tidligere versjoner som er ikke lenger tilgjengelige

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 732 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf